Indentation force-deflection is a process used in the flexible foam manufacturing industry to assess the "softness" of a sample of foam such as memory foam. To conduct an IFD test, a circular flat indenter with a surface area of 323 square centimeters (50 sq. inches - 8" in diameter) is pressed against a foam sample usually 100 mm thick and with an area of 500 mm by 500 mm (ASTM standard D3574). The foam sample is first placed on a flat table perforated with holes to allow the passage of air. It is then "warmed up" by being compressed twice to 75% "strain", and then allowed to recover for six minutes. The force is measured 60 seconds after achieving 25% indentation with the indenter. Lower scores correspond with less firmness; higher scores with greater firmness. US measurements are given

Property Value
dbo:abstract
  • Indentation force-deflection is a process used in the flexible foam manufacturing industry to assess the "softness" of a sample of foam such as memory foam. To conduct an IFD test, a circular flat indenter with a surface area of 323 square centimeters (50 sq. inches - 8" in diameter) is pressed against a foam sample usually 100 mm thick and with an area of 500 mm by 500 mm (ASTM standard D3574). The foam sample is first placed on a flat table perforated with holes to allow the passage of air. It is then "warmed up" by being compressed twice to 75% "strain", and then allowed to recover for six minutes. The force is measured 60 seconds after achieving 25% indentation with the indenter. Lower scores correspond with less firmness; higher scores with greater firmness. US measurements are given in pounds-force, and European ones are given in newtons. (en)
dbo:wikiPageExternalLink
dbo:wikiPageID
  • 42387402 (xsd:integer)
dbo:wikiPageLength
  • 1625 (xsd:nonNegativeInteger)
dbo:wikiPageRevisionID
  • 1070455469 (xsd:integer)
dbo:wikiPageWikiLink
dbp:wikiPageUsesTemplate
dcterms:subject
gold:hypernym
rdf:type
rdfs:comment
  • Indentation force-deflection is a process used in the flexible foam manufacturing industry to assess the "softness" of a sample of foam such as memory foam. To conduct an IFD test, a circular flat indenter with a surface area of 323 square centimeters (50 sq. inches - 8" in diameter) is pressed against a foam sample usually 100 mm thick and with an area of 500 mm by 500 mm (ASTM standard D3574). The foam sample is first placed on a flat table perforated with holes to allow the passage of air. It is then "warmed up" by being compressed twice to 75% "strain", and then allowed to recover for six minutes. The force is measured 60 seconds after achieving 25% indentation with the indenter. Lower scores correspond with less firmness; higher scores with greater firmness. US measurements are given (en)
rdfs:label
  • Indentation force-deflection (en)
owl:sameAs
prov:wasDerivedFrom
foaf:isPrimaryTopicOf
is dbo:wikiPageRedirects of
is dbo:wikiPageWikiLink of
is foaf:primaryTopic of
Powered by OpenLink Virtuoso    This material is Open Knowledge     W3C Semantic Web Technology     This material is Open Knowledge    Valid XHTML + RDFa
This content was extracted from Wikipedia and is licensed under the Creative Commons Attribution-ShareAlike 3.0 Unported License